What are the testing facilities available at KARAM?

KARAM only follow EDANA (ERT) References for testing. Equivalent other International references are also mentioned

EST EDANA INDA ASTM ISO
Tensile Strength ERT 20.2-89 IST 110.4-95 D 5035-95 ISO 9073-3:1989
Thickness ERT 30.5-99 IST 120.1 ISO 9073-2: 1995(E)
Weight ERT 40.3-90 IST 130.1 D 3776-96 ISO 9073-1: 1989
Tear Strength ERT 70.4-99 IST 100.2-95 D 5733-95 ISO 9073-4: 1997
Air Permeability ERT 140.1-99 IST 70.1 D 737-96 ISO 9237:1995
Liquid Strike Through ERT 150.4-99 IST 70.3-98 ISO 9073-8: 1995